Sign In | Join Free | My udpf.com |
|
Brand Name : YUHONG
Model Number : ASTM B111 C70600
Certification : ABS, GL, DNV, NK, PED, AD2000, GOST9941-81, CCS, ISO 9001-2008
Place of Origin : CHINA
MOQ : 100KGS
Price : Negotiable
Payment Terms : L/C,T/T
Supply Ability : 1000Tons/Month
Delivery Time : 7DAYS
Packaging Details : Ply-wooden Case /Iron Case/ Bundle with plastic Cap
Standard : ASTM B111/ASME SB111
Material : Copper Nickel Alloy C70600
Length : 3000mm-6000mm, 6 Meters Or Customized, 18000max., 11.8m Or As Required., 8m
Thickness : 0.4-30mm, 1.0mm, 0.6mm-2500mm, 1mm-60mm, 0.6-25 Mm
Outer Diameter : 6-630mm, Customized, 6-762mm, 6-860mm;, 6mm-630mm
Surface : Annealing, 8K, Polishing Or Unpolishing, Morror/Satin
Application : Heat Exchanger/Boiler/Condenser/Chemical
ASTM B111 C70600 O61 Copper Nickel Alloy Low Fin Tube For Heat Exchanger
In the ASTM B111/B111M-18 standard, the requirements for C70600 white copper tube BFe10-1-1 heat exchange tube are very strict. Among them, there are detailed regulations on the composition, structure, performance, size, and shape of materials. The EN12451 standard proposes corresponding execution standards for the European market, mainly including chemical composition, physical properties, mechanical properties, non-destructive testing, and other aspects.
In addition to the above two standards, there are also relevant domestic standards, such as GB/T 8890-2018, which have strict regulations on the material appearance, composition, mechanical properties, dimensional tolerances, and other aspects of C70600 white copper tube BFe10-1-1 heat exchange tube.
In summary, the implementation of standards is crucial for the quality control, performance evaluation, and technical application of C70600 white copper tube BFe10-1-1 heat exchange tube. Enterprises must strictly follow the standards during the production process to ensure product quality.
C70600 white copper tube
Due to its excellent corrosion resistance, white copper is mainly used in key industrial fields such as seawater desalination evaporation pipes, central air conditioning condenser pipes, ship air coolers, petrochemical coolers, and power plant steam turbine condensers. White copper is a copper based alloy with nickel as the main additive element, which is silver white and has a metallic luster, hence the name white copper. Copper and nickel can dissolve each other infinitely to form a continuous Solid solution, that is, regardless of the proportion of each other α-- Single phase alloy. When nickel is melted into red copper with a content of D200 exceeding 16%, the resulting alloy becomes relatively white like silver in color. The higher the nickel content, the whiter the color. However, after all, it blends with copper. As long as the nickel content ratio does not exceed 70%, the yellow color of copper can be seen with the naked eye. Moreover, the nickel content in white copper is usually 25%.
C70600 copper nickel alloy has excellent corrosion resistance to clean or polluted seawater and river water, and is widely used in heat exchangers that use seawater in power plants, desalination, petrochemical plants, and other industries.
C70600 Copper Nickel Tube Heat Exchanger Tube Chemical Composition
C70600 Chemical Composition | DIN 86019 | EEMUA 144 | BS 2871 | ASTM B466 | JIS H 3300 | MIL-T-16420K |
Ni% | 9.0-11.0 | 10.0-11.0 | 10.0-11.0 | 9.0-11.0 | 9.0-11.0 | 9.0-11.0 |
Fe% | 1.5-1.8 | 1.5-2.0 | 1.0-2.0 | 1.0-1.8 | 1.0-1.8 | 1.0-1.8 |
Mn% | 0.5-1.0 | 0.5-1.0 | 0.5-1.0 | Max.1.0 | 0.2-1.0 | Max.1.0 |
C% | Max0.05 | Max0.05 | Max0.05 | Max0.05 | Max0.05 | |
Pb% | Max0.03 | Max0.01 | Max0.01 | Max0.02 | Max0.05 | Max0.02 |
S% | Max0.015 | Max0.02 | Max0.05 | Max0.02 | Max0.02 | |
P% | Max0.02 | Max0.02 | Max0.02 | Max0.02 | ||
Zn% | Max0.15 | Max0.20 | Max0.50 | Max0.50 | Max0.05 | |
Zr% | Max0.03 | |||||
Others | Max0.30 | Max0.30 | Max0.30 | |||
Cu% | Balance | Balance | Balance | Balance | Cu+Ni+Fe+MnMin.99.5 | Min.86.5 |
C70600 Copper Nickel Tube Heat Exchanger Tube Mechanical Properties
Properties | Metric | Imperial |
Tensile strength,ultimate | 303-414 MPa | 43900-60000 psi |
Tensile strength,yield(depending on temper) | 110-393 MPa | 16000-57000 psi |
Elingation at break(in 254 mm) | 42.00% | 42.00% |
Machinability(UNS C36000(free-cutting brass)=100%) | 20% | 20% |
Shear modulus | 52.0 GPa | 7540 ksi |
Poisson's ratio | 0.34 | 0.34 |
Elastic modulus | 140 GPa | 20300 ksi |
![]() |